合金C276哈氏合金是镍铬钼合金的一种变体。它还有各种各样的附加功能。加入钨使这种合金具有强度。它是一种高度耐腐蚀的合金。钼和镍的含量使合金具有很高的抗点蚀性。哈氏C276 UNS N10276中铬的含量使其具有抗氧化介质的能力。该合金在焊接过程中的碳化物析出非常少,因为成分中的碳含量非常少。在哈氏合金中,DIN 2.4819材料具有最佳的强度、耐腐蚀性和成本效益。因此,它是最广泛使用的变体。哈氏C276价格实惠。 You can contact us for a full price list. The properties such as the Hastelloy C276 density, pressure ratings, strength, thermal conductivity and the corrosion resistance makes it applicable along a wide range of applications. There are different types of products in this material. The Hastelloy C276 suppliers produce bars, sheets, plates, tubes and pipes, pipe fittings and welding wires from this material. The material has resistance against wet chlorine gas, chlorine dioxide and hypochlorite. It is resistant to corrosion in welded joints as it minimizes the intergranular precipitation during welding. The resistance to reducing agents is significant. The alloy is resistant to strong oxidizing agents such as salts. All of these mechanical properties are due to the specific chemical mixture. The哈氏C276化学组成有镍、钼、铬、铁、钨、螺杆、锰、碳、钒、磷、硅、硫等。该材料用于燃料气体脱醇系统、含硫气井、纸浆和造纸工业、废水处理和污染控制系统。哈氏C276的等效材料并不多,但哈氏C276的其他等级有时可以被用来代替哈氏C276。
合金C276价格 | 40美元/公斤 |
UNS编号:N10276
W.Nr。数量(DIN): 2.4819
HASTELLOY®c - 276合金 (N10276 W10276) |
|
片材、板材和带材 | B 575 / SB 575 P = 43 |
---|---|
钢坯、棒材和棒材 | B 574 / SB 574 P = 43 |
药皮焊条 | SFA 5.11/ A 5.11 (ENiCrMo-4) DIN 2.4887 (EL-NiMo15Cr15W) F = 43 |
焊条及焊丝裸露 | SFA 5.14/ A 5.14 (ERNiCrMo-4) DIN 2.4886 (SG-NiMo16Cr16W) F = 43 |
无缝管 | B 622 / SB 622 P = 43 |
焊接的管道 | B 619 /SB 619 P = 43 |
管件 | B 366 / SB 366 P = 43 |
锻造产品 | B 564 / SB 564 P = 43 |
喧嚣 | 17744号2.4819 NiMo16Cr15W |
德国莱茵 | Werkstoffblatt 400 Kennblatt 320 Kennblatt 319 |
其他Stanard | NACE MR0175 ISO 15156 |
爹妈 | 在 | 材料NR (WNR)。 | 使用其 | JIS | 废话 | GOST |
---|---|---|---|---|---|---|
N10276 | NiMo16Cr15W | 2.4819 | - - - - - - | 0276年西北 | - - - - - - | ХН65МВУ |
HASTELLOY®c - 276合金 (W10276 / N10276) |
|||
ASME | l节 | 1000°F(538°C) 1 | |
---|---|---|---|
节大典时 | 类1 | - | |
二班 | 800°F(427°C) 2 | ||
3班 | 800°F(427°C) 2 | ||
部分Vlll | Div。 | 1250°F(677°C) 3 | |
Div。 | 1250°F(677°C) 3 | ||
部分Xll | 650°F(343°C) 3 | ||
B16.5 | 1250°F(677°C) 4 | ||
B16.34 | 1250°F(677°C) 5 | ||
B31.1 | 1000°F(538°C) 6 | ||
B31.3 | 1250°F(677°C) 7 | ||
VdTUV (doc #) | 844°F(450°C) 8, # 400 |
年级 | % | 倪 | W | Cr | 菲 | 有限公司 | C | 莫 | 锰 | 年代 | 如果 | V | P |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
C | 分钟。 |
平衡 | 3. | 14.5 | 4 | 15 | |||||||
Max。 | 4.5 | 16.5 | 7 | 2.5 | 0.08 | 17 | 1 | 0.03 | 1 | 0.35 | 0.04 | ||
C276 | 分钟。 | 平衡 | 3. | 14.5 | 4 | 15 | |||||||
Max。 | 4.5 | 16.5 | 7 | 2.5 | 0.01 | 17 | 1 | 0.03 | 0.08 | 0.35 | 0.04 |
物理性质
密度 | 8.9 g / cm³ |
熔点 | 1325 - 1370℃ |
合金状态 | 屈服强度rp0。2 n /毫米² | 抗拉强度 Rm N /毫米² |
伸长 5%的 |
C / C276 | 283 | 690 | 40 |
优良的耐腐蚀材料